EMS-Grivory Grilamid® XE 3771 Nylon 12, 95% Polymer XE 3771+ 5% Polymer XE 3772
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Polymer XE 3771 is the cross linkable grafted copolymer. Polymer XE 3772 is the catalyst masterbatch which accelerates the cross linking. This two grades are used as blend for the inner layer of the patented EMS-CHEMIE Coolant System hose structure "ECOSYS“.Information provided by EMS-Grivory
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Unnotched
- Izod Impact, Notched
- Melting Point
|
|
|
|