EMS-Grivory Grilamid® XE 3835 Black 9992 Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid XE 3835 black 9992 is a medium viscosity extrusion grade Polyamide 12 (PA 12). Grilamid XE 3835 black 9992 is heat stabilized and impact modified. Grilamid XE 3835 black 9992 is suitable for the extrusion of profiles and tubes for applications in automotive fuel system and in industrial markets. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Head Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|