EMS-Grivory Grilamid® XS 04_01 Black Nylon 12, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Grilamid XS 04_01 Black is a 23% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade.Information provided by EMS-Grivory
| Available Properties |
- Density
- Melt Flow
- Ash
- Tensile Strength at Break
- Flexural Modulus
- Melting Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|