EMS-Grivory Grilon® A70GF30H Nylon 66, 30% Glass Fiber Filled, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Grilon A 70 GF 30 H is a 30% glass fiber reinforced nylon 6.6 injection molding grade. It offers high rigidity and heat deflection temperature plus outstanding resistance to heat and weathering. The processing characteristics of Grilon A 70 GF 30 H are excellent and it offers the high chemical resistance typical of nylons. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Strength
- Comparative Tracking Index
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|