EMS-Grivory Grilon® A 28 Nylon 6, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Grilon A 28 is an unreinforced, standard PA6 injection molding grade with normal melt viscosity. Grilon A 28 has wide variety of applications in all market sectors, automotive, electrical, leisure and sport, e. g. clips, covers, housings. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
- Hold Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|