EMS-Grivory Grilon® AG-30 LF15 Black 9832 Nylon 66, 30% Glass Fiber, 15% PTFE and Silicon Filled, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Grilon AG-30 LF 15 black 9832 is a normal viscosity, heat stabilized PA66-moulding type with 30% glass fiber reinforcement and 15% of a combination PTFE and silicon oil.Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Melting Point
- Flammability, UL94
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
- Hold Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|