EMS-Grivory Grilon® XE 3748 Black 9210 Nylon 6, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Grilon XE 3748 Black 9210 is a nylon 6 elastomer with very high flexibility. It is heat stabilized, extrusion blow moldable and has a high impact strength even at low temperatures. Due to its high melt strength, Grilon XE 3748 is particularly well suited for the production of extrusion blow molded articles. It is processable on conventional as well as on 3 D-machines. This product is well suited for use as the flexible part in sequential blow molding in conjunction with a rigid nylon 6 such as: Grilon EB 50 HDZ, Grilon R50 HNZ or Grilon RVZ-15H.1 Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Feed Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|