EMS-Grivory Grilon® XS 03_0002 Natural Nylon 6, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Grilon XS 03_0002 Natural is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon XS 03_0002 Natural is used typically for co-extruded fuel lines, coolant pipes in deep freezer units, vulcanization mandrels, and vacuum lines. Information provided by EMS-Grivory
| Available Properties |
- Density
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Processing Temperature
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Head Temperature
- Drying Temperature
- Dry Time
|
|
|
|