EMS-Grivory Grivory® HB FE 5299 Natural Nylon Copolymer, As Conditioned
Subcategory: Nylon; Thermoplastic
Material Notes: FE5299 natural is a lactam free, lubricated Copolyamide material targeted for demanding multilayer high barrier structures.Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Water Vapor Transmission
- Oxygen Transmission
- Carbon Dioxide Transmission
- Thickness
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tear Strength Test
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Melting Point
- Processing Temperature
- Adapter Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|