EMS-Grivory Grivory® HT FE 5643 white L00354.12 Partially Aromatic Nylon, 33% Glass Fiber Filled, Dry as Molded
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic
Material Notes: Grivory HT FE5643 white is a new high heat stabilized 33 wt.-% glass fiber reinforced injection molding grade based on a semi crystalline partially aromatic polyamide.Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Hold Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|