EMS-Grivory Grivory® HB FE 5793 Partially Aromatic Nylon
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic
Material Notes: Grivory HB FE5793 is a processing stabilized version of Grivory HB FE4581.Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission
- Carbon Dioxide Transmission
- Thickness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Melting Point
- Glass Temperature
- Processing Temperature
- Adapter Temperature
- Die Temperature
|
|
|
|
| Property Data |