EMS-Grivory Grivory® HT1V-4 FA Black 9225 Partially Aromatic Nylon, 40% Glass Fiber Filled, Dry as Molded
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer
Material Notes: Grivory HT1V-4 FA black 9205 is a 40% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance values at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. Grivory HT1V-4 FA black 9225 is suitable for all thermoplastic applications with the requirement of FDA approval. According to FDA (Food and Drug Administration) Grivory HT1V-4 FA black 9225 is approved for contact with all foodstuffs at all temperatures, without limitations. Grivory HT1V-4 FA black 9225 also satisfies the EU guidelines (EU Directive 02/72) for materials in contact with foodstuffs. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
- Hold Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|