EMS-Grivory Grivory® XE 3671 Partially Aromatic Nylon, 50% Glass Fiber Filled, Dry as Molded
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer
Material Notes: Grivory XE 3671 is a heat stabilized, 50 % glass fiber reinforced, partially aromatic polyamide for injection molding. Grivory XE 3671 is a development product which shows a significantly improved impact and notched impact strength in comparison to Grivory GV-5H. In general, polyamides show a reduction in stiffness and strength through water absorption. In Grivory products, this has been reduced by the partially aromatic matrix. As well as all Grivory products, XE 3671 is resistant against a wide rage of chemicals and oils. Information provided by EMS-Grivory
| Available Properties |
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|