EMS-Grivory Grivory® XE 3706 Partially Aromatic Nylon, 60% Glass Fiber Filled, Dry as Molded

 

Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer

Material Notes:
Grivory XE 3706 is a 60% glass fiber-reinforced, partially aromatic polyamide designed for die cast metal replacement. Grivory GV grades have very low warpage and high stiffness and strength (high tensile strength and high flexural modulus). They also have excellent dimensional stability, meaning that the mechanical properties are virtually unaffected by humidity.

Grivory Super stiff exhibits good injection moldability and surface finish, an unusual trait for materials with such high glass loadings. Grivory GV grades also exhibit less tool abrasion than other comparably filled nylons. Like most nylons, Grivory has good chemical resistance.

Information provided by EMS-Grivory

Available Properties
  • Density
  • Water Absorption
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Izod Impact, Notched @ -40°C
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。