EMS-Grivory Grivory® XE 3713 Partially Aromatic Nylon, 45% Glass Fiber Filled, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer
Material Notes: Grivory XE 3713 is a heat stabilized, 45% glass fiber reinforced, partially aromatic polyamide for injection molding. Compared to Grivory GV-5H, Grivory XE 3713 shows an improved UV-resistance. In general, polyamides show a reduction in stiffness and strength through water absorption. In Grivory, Grivory XE 3713s, this has been reduced by the partially aromatic matrix. As well as all Grivory, Grivory XE 3713 is resistant against a wide rage of chemicals and oils. Information provided by EMS-Grivory
| Available Properties |
- Water Absorption
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|