EMS-Grivory Grivory® XE 3728 Partially Aromatic Nylon, 60% Glass Fiber Filled, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer
Material Notes: Grivory XE 3728 black 9915 is a heat stabilized, 60 % glass-fiber reinforced, partially aromatic polyamide for injection molding. Grivory XE 3728 black 9915 is a development product which shows an improved flow ability and surface finish in comparison to Grivory GV-6H. Information provided by EMS-Grivory
| Available Properties |
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|