EMS-Grivory Grivory® TR XE 3805 Transparent Nylon, As Conditioned
Subcategory: Nylon; Thermoplastic
Material Notes: Grivory TR XE 3805 is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grivory TR XE 3805 offers outstanding properties. Grivory TR XE 3805 is a dedicated material for high quality optical lens applications. Lenses manufactured out of Grivory TR XE 3805 are in compliance with the Optical Class 1 Standard. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Ball Indentation Hardness
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Flammability, UL94
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
- Hold Pressure
- Back Pressure
- Screw Speed
- Abbe Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|