EMS-Grivory Grivory® XS 1363 Partially Aromatic Nylon, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer
Material Notes: Grivory XS 1363 is a 50% glass fiber reinforced, partially aromatic nylon. Designed specifically for the aircraft industry. Grivory XS 1363 exhibits good injection moldability and less tool abrasion than other comparably filled nylons. Like most nylons, Grivory XS 1363 has good chemical resistance. Using Grivory XS 1363 instead of aluminum or magnesium offers many advantages; lower weight, corrosion free and little or no finishing (cleaning, machining, deflashing, painting, etc). In addition, tool life span for Grivory is greater than that of a metal die cast tool. These advantages over die cast metals lead to lower production costs, typically between 20 and 50 percent. Grivory XS 1363 is suitable for use in interior aircraft cabin applications. Its high strength and stiffness is virtually unaffected by moisture , this combined with a good surface finish makes it ideal for applications such as: armrests, spreaders, tray brackets, overhead bin brackets, etc. Information provided by EMS-Grivory
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|