EMS-Grivory Grilamid EA 20 HV1 Unreinforced Nylon 12 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Description: It is the adhesive layer between Grilpet B24 HNZ or Grilpet B24 ESD and Grilamid L25 W40 X. It exhibits high adhesive strength to all of the above mentioned products Application Examples: Tube construction for high barrier fuel lines. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
|
|
|
|