EMS-Grivory Grilamid L16 G Unreinforced Nylon 12 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Description: Lower viscosity, high flow, fast cycling grade and offers low moisture absorption, excellent dimensional stability. It is lubricated and heat stabilized. Easy processing. Application Examples: Applications where high production rates are demanded and for parts with complex shapes or very long flow paths. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Zone 5
- Die Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|