EMS-Grivory Grilamid L20 ANZ Unreinforced Nylon 12 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Description: High viscous extrusion blow molding grade with good melt strength, exceptionally good hydrolytic stability, exhibits unusually good resistance to zinc chloride, hot water and antifreeze solutions. It has a high impact strength even at low temperatures. Application Examples: Designed for automotive applications, e.g. flexible gas filler necks or rigid pipes for automotive cooling systems. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Zone 5
- Die Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|