EMS-Grivory Grilamid L25 W40 X Unreinforced Nylon 12 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 12
Material Notes: Description: High viscosity extrusion grade, flexible, excellent impact properties even at low temperatures. Heat and UV stabilized, very easy to process. Automotive Approvals: - Chrysler MS-DB467
- Ford WSK-M4D701-A (black9992, natural6504)
- GM GMP PA12.003
Application Examples: Flexible pipes for pneumatic, gas and oil lines in automotive and engineering industries. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Izod Impact, Notched @ -18°C
- Izod Impact, Notched @ -40°C
- Volume Resistivity
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Zone 5
- Die Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|