EMS-Grivory Grivory G16 Partially Aromatic Film Grade Nylon

 

Subcategory: Nylon; Thermoplastic; Nylon, Aromatic; Polymer

Material Notes:
Description: Partially aromatic nylon, fulfils EU and FDA requirements for direct contact with foodstuff. For blown and cast film. Suitable for extrusion blow molding and injection blow molding. Outstanding oxygen barrier, particularly in very damp conditions. Good barrier properties flavor and odor, good transparency. Greater rigidity than nylon 6, even after water absorption. Listed under FDA Regulations CFR21 paragraph 177.1500 (Natural only).

Application Examples: Transparent, hollow vessels, packaging films, deep-drawn plates

Data provided by EMS-Grivory.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Moisture Vapor Transmission
  • Oxygen Transmission
  • Nitrogen Transmission
  • Carbon Dioxide Transmission
  • Melt Flow
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Break, MD
  • Film Elongation at Break, MD
  • Film Elongation at Yield, MD
  • Tensile Modulus
  • Tear Strength Test
  • Dart Drop Total Energy
  • Glass Temperature
  • Gloss
  • Processing Temperature
  • Adapter Temperature
  • Die Temperature
  • Damaging Deformation
  • Damaging Force
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。