EMS-Grivory Grivory GTR 45 Partially Aromatic Nylon (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic
Material Notes: Description: Transparent, partially aromatic nylon, good rigidity in a conditioned state. Fulfills EU and FDA regulations for direct contact with non-alcoholic foodstuff. Listed under ANSI / NSF Standard 61 (Natural & Black only). Application Examples: Transparent injection molded parts which require chemical and scratch resistance, but are not exposed to UV light. Sight lenses, light switches, reservoirs Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Refractive Index
- Transmission, Visible
- Processing Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Melt Temperature
- Mold Temperature
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|