EMS-Grivory Grivory GM-4H 40% Mineral Filled Nylon (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: Description: Injection molding grade reinforced with 40% mineral content, heat stabilized, isotropic injection shrinkage, outstanding surface quality, high stiffness, even in a conditioned state, shrinkage similar to that of die-cast alloys Application Examples: Visible parts with high requirements on the surface quality. Geometrically demanding functional parts Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|