EMS-Grivory Grivory HTM-4H1 High Temperature 40% Mineral Reinforced Nylon (Conditioned)
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: Description: Injection molding grade based on copolymers nylon 6T/6I, reinforced with 40% mineral content. Stiff and stable even at application temperatures of up to 248°F, heat stabilized. Exhibits low distortion, dimensionally stable, low thermal expansion. Can be electro-plated. Approved to ANSI / NSF Standard 61 (Natural & Black only), KTW for cold and hot water applications up to 90°C, and WRC for cold and hot water applications up to 85°C. Application Examples: Stiff, technical components with low distortion, good dimensional stability and low thermal expansion. Functional and visible parts with electro-plated surfaces. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Feed Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|