EMS-Grivory Grilon A23 Unreinforced, Low Viscosity Nylon 6 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: Injection molding grade (nylon 6) with low viscosity, also suitable for extrusion, FDA Regulations CFR21 paragraph 177.1500 (Direct contact) listed. Application Examples: For compounding of high-flow injection molding grades, or specialized extrusion application Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Die Temperature
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|