EMS-Grivory Grilon R47 HW 10 Unreinforced, High Viscosity, Flexural Modified Nylon 6 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: High viscosity, flexural-modified grade of nylon 6. Stabilized for protection against both thermal and UV degradation. It offers excellent strength, toughness, ductility and abrasion resistance, and provides very good resistance to a wide range of chemicals, solvents, oils and greases. Automotive Approvals: ASTM D4066 PA261 Application Examples: Applications where flexibility and toughness are required, flexible tubing for automotive and industrial applications. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Nozzle Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|