EMS-Grivory Grilon R47 NZE Unreinforced, High Viscosity, Impact Modified Nylon 6 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: High viscosity, flexural modified grade of (nylon 6) for extrusion and injection molding. Heat and UV stabilized, exceptional strength, toughness, ductility, and abrasion resistance, as well as very good resistance to a range of chemicals, solvents, oils and greases. Automotive approvals: Chrysler MS-DB41 CPN3821, GM GMP.PA6.037, ASTM D4066 PA0261, ASTM D4066 PA251 Application Examples: flexible tubing for air conditioning units, paint spraying and high pressure cleaning equipment. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Nozzle Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|