EMS-Grivory Grilon EBV-15H 15% Glass Reinforced Nylon 6 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: High viscosity, impact modified extrusion blow molding material, 15% glass fibers reinforced, heat stabilized, easy processing, good toughness also at low temperatures. Automotive approvals: ASTM D4066 PA0200 G15 A29590 UA035 YG150 Application Examples: Air duct parts, door handles. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Feed Temperature
- Zone 1
- Zone 2
- Zone 3
- Adapter Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|