EMS-Grivory Grilon PV-3H 30% Glass Reinforced Nylon 6 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: 30% glass fiber reinforced nylon 6 resin, which exhibits excellent mechanical properties, strength, rigidity and toughness. It is resistant to a wide range of chemicals, solvents, oils and greases and provides excellent long term thermal stability. Listed under FDA Regulations CFR21 paragraph 177.1500 (Direct contact). Application Examples: Where high levels of practical toughness are required. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|