EMS-Grivory Grilon PV-35H 35% Glass Reinforced Nylon 6 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: 35% glass fiber reinforced nylon 6 resin, that exhibits excellent mechanical properties, strength, high rigidity and toughness. It is resistant to a wide range of chemicals, solvents, oils and greases and provides excellent long term thermal stability. Listed under FDA Regulations CFR21 paragraph 177.1500 (Direct contact). Application Examples: Where high levels of practical toughness are required. Data provided by EMS-Grivory.
|
|
|
| Property Data |