EMS-Grivory Grilon PV-3H HM 30% Glass Reinforced, Injection Molding Grade Nylon 6 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Injection molding grade (nylon 6) reinforced with 30% glass fiber, specially developed for injection molding bonding processes with thermoplastic elastomers in the shore A range of SEBS-copolymers and PP/EPDM. UL listed. Application Examples: Automotive components such as connectors, covers for rear wipers, IR automobile key, steering column switches. Electro-components such as switch knobs, handles or applications with molded-on seals. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|