EMS-Grivory Grilon PVN-3H Impact Modified, 15% Glass Fiber Reinforced Nylon 6 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Impact modified, 30% glass fiber reinforced nylon 6 resin for injection molding. It exhibits excellent mechanical properties, a combination of strength, rigidity and toughness and is resistant to a wide range of chemicals, solvents, oils and greases. Application Examples: Applications where high levels of practical toughness are required, especially in dry conditions. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Comparative Tracking Index
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|