EMS-Grivory Grilon TV-3H 30% Glass Fiber Reinforced Nylon 66 (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: Description: 30% glass fiber reinforced nylon 66 injection molding resin. It offers good rigidity and heat deflection temperature plus outstanding resistance to high heat and weathering. It has excellent processing characteristics and high chemical resistance. Application Examples: electrical bobbins, switches, sockets, housings, fan blades, automotive clips, handles, levers, appliance components, power tool housing and internal parts. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|