EMS-Grivory Grilon TS VO Flame Retardant Tailor Made Nylon 6/Nylon 66 Alloy (Dry as Molded)
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: Flame retardant tailor made alloy of nylon 66 and nylon 6 combined with additives for improved processability and heat resistance. It has an ideal combination of stiffness and impact strength and caters for injection molding applications requiring excellent surface finish. Application Examples: Applications where good flowability and excellent surface finish is needed in industries such as automotive, under hood applications, electro and electronics, safety technology, mechanical engineering and domestic applications. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched @ -30°C
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Comparative Tracking Index
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|