MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

EMS-Grivory Grilamid LV-2A NZ 20% Glass Reinforced Nylon 12 (Dry as Molded)

 

Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer

Material Notes:
Description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with a 20% glass fiber content which is hydrolytic resistant, extrusion blow moldable and has a high impact strength even at low temperatures. Due to its very high melt strength, Grilamid LV-2A NZ is particularly well suited for the production of extrusion blow molded articles, especially for large parts. It is processable on conventional as well as on 3 D-machines. Grilamid LV-2A NZ is characterized by excellent resistance to most of the media used in automobiles, in particular by its resistance to zinc chloride solutions. In addition the material exhibits an unusually good resistance to hot water and antifreeze solutions. This product is suitable for technical articles of all kinds, especially for applications in the automotive industry.

Data provided by EMS-Grivory.

Available Properties
  • Specific Gravity
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • CTE, linear 20°C
  • CTE, linear 20°C Transverse to Flow
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Deflection Temperature at 8.0 MPa
  • Flammability, UL94
  • Processing Temperature
  • Feed Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Head Temperature
  • Drying Temperature
  • Dry Time
  • Dew Point
  • Hopper Zone
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。