EMS-Grivory Grilamid LV-2A NZ 20% Glass Reinforced Nylon 12 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with a 20% glass fiber content which is hydrolytic resistant, extrusion blow moldable and has a high impact strength even at low temperatures. Due to its very high melt strength, Grilamid LV-2A NZ is particularly well suited for the production of extrusion blow molded articles, especially for large parts. It is processable on conventional as well as on 3 D-machines. Grilamid LV-2A NZ is characterized by excellent resistance to most of the media used in automobiles, in particular by its resistance to zinc chloride solutions. In addition the material exhibits an unusually good resistance to hot water and antifreeze solutions. This product is suitable for technical articles of all kinds, especially for applications in the automotive industry. Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Processing Temperature
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Head Temperature
- Drying Temperature
- Dry Time
- Dew Point
- Hopper Zone
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|