EMS-Grivory Grilamid LV-2H 20% Glass Reinforced, Heat Stabilized Nylon 12 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Description: Grilamid LV-2H is a 20% glass reinforced, heat stabilized nylon 12 injection molding grade with good chemical resistance, good UV stability, high impact strength, conforms to UK WRAS drinking water standards, very dimensionally stable. Application Examples: Electro, Electronics, Automotive, Safety Technology, Mechanical Engineering, Domestic Appliances Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Processing Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Dew Point
- Hold Pressure
- Screw Speed
- Clamping Force
- Dynamic Pressure
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|