EMS-Grivory Grilamid TR 90 LX Transparent Nylon (Conditioned)
Subcategory: Nylon; Thermoplastic
Material Notes: Description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 LX is characterized by its extremely good UV resistance, high chemical and stress crack resistance as well as high impact strength. Application Examples: Optic, Electro / Electronics, Automotive, Mechanical engineering, Domestic appliances, Sanitary Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Ball Indentation Hardness
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Processing Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Dew Point
- Hold Pressure
- Screw Speed
- Clamping Force
- Dynamic Pressure
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|