EMS-Grivory Grilon BR 40 W Extrusion Grade Nylon 6 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W characterizes itself through the following properties: High flexibility, high impact strength. Application Examples: extrusion applications such as flexible tubes Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Head Temperature
- Drying Temperature
- Dry Time
- Dew Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|