EMS-Grivory Grilon FG 40 NL Natural 6021 Film Grade Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Grilon FG 40 NL nat 6021 is a modified, high viscosity polyamide 6, suitable for production of mono or coex blown and cast film. As a result of the modification it offers in comparison to conventional polyamide 6 following improvements: better gas barrier properties at elevated humidity and after pasteurization and sterilization, improved optical and UV-light absorption properties, better aroma barrier and flavor. Application Examples: oriented films, sausage casings, deep drawn films, meat cheese packaging, fish (pouches, shells, covers) Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Water Vapor Transmission
- Oxygen Transmission Rate
- Carbon Dioxide Transmission
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Tensile Modulus
- Coefficient of Friction
- Tear Strength
- Tear Strength, Total
- Melting Point
- Gloss
- Processing Temperature
- Zone 1
- Zone 2
- Zone 3
- Adapter Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Dew Point
- 900 Cycle Gelbo Flex Tester
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|