EMS-Grivory Grilon TSS/4 LF 20 20% PTFE and Silicon Filled Nylon 6/Nylon 66 Blend (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Grilon TSS/4 LF 20 is a heat stabilized, normal viscosity PA66 and PA6 injection molding grade with 20% lubricant (PTFE & Silicon). Grilon TSS/4 LF 20 characterizes itself through the following properties: exceptional bearing properties, low abrasion. Application Examples: pump pistons, sliding components, slide rings, and slide levers Data provided by EMS-Grivory.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Processing Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Dew Point
- Hold Pressure
- Screw Speed
- Clamping Force
- Dynamic Pressure
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|