EMS-Griltech Grilon® KA 140 White CoPA Fiber
Subcategory: Nylon; Thermoplastic
Material Notes: Description: GRILON KA 140 is the standard homo component fusible adhesive fiber. CoPA fiber is characterized by a wide processing window and high adhesive strength. Data provided by EMS-Griltech.
| Available Properties |
- Fiber Count
- Melt Temperature
- Color
- Luster
- Staple Length
|
|
|
|