PolyOne Catize® DLPZ-1 Inherently Conductive Polymer/metal mixtures
Subcategory: Additive/Filler for Polymer; Thermoplastic; Polymer
Material Notes:
Description/Features: - A mixture of an Inherently Conductive Polymer and metal particles.
Applications: - Coil coating
- Industrial maintenance coatings
- Marine Coatings
- OEM coatings
- Rebar & Bridge Coatings
- Fastener Coatings
As with any dry pigment, we do not recommend post adding Catize to a finished coating unless it is pre-dispersed in a suitable carrier. Catize should be added early on in the grind to ensure proper dispersion. Disclaimer: Catize corrosion control additives are made under license of GeoTech's U.S. Pat. Nos. 5,976,419; 6,231,789; 6,440,332; 6,627,117 and other patents pending. Catize has been tested in several finished coating formulations. It performs better on non-pretreated surfaces. Adequate cure time should be allowed prior to accelerated corrosion testing. Topcoating is not required for excellent salt spray results. Information provided by PolyOne Corporation.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|