PolyOne Catize® WBP-3 Inherently Conductive Polymer/metal mixtures

 

Subcategory: Additive/Filler for Polymer; Thermoplastic; Polymer

Material Notes:

Description/Features:

  • A mixture of an Inherently Conductive Polymer and metal particles.

Applications:

  • Coil coating
  • Industrial maintenance coatings
  • Marine Coatings
  • OEM coatings
  • Rebar & Bridge Coatings
  • Fastener Coatings

Processing Method:

  • Can be processed with normal dispersing equipment, such as high speed dispersers
  • for optimal results, contact PolyOne's technical staff to determine recommended processing.

Catize WBP-3 has been tested in several finished coating formulations as a post-add additive. It performs better on non-pretreated surfaces. Adequate cure time should be allowed prior to accelerated corrosion testing. Topcoating is not required for excellent salt spray results.

Disclaimer: Catize corrosion control additives are made under license of GeoTech's U.S. Pat. Nos. 5,976,419; 6,231,789; 6,440,332; 6,627,117 and other patents pending.

Information provided by PolyOne Corporation.

Available Properties
  • Solids Content
  • Particle Size
  • Color
  • Inherently Conductive Polymer Type
  • Metal Particle type
  • Product Form
  • Salt Spray
  • Scanning Vibrating Electrode (SVET)
  • Solvent Type
  • Tafel Plot
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。