PolyOne ECCOH™ 0521-48 Low Smoke Free Of Halogen (LSFOH)
Subcategory: Thermoplastic
Material Notes:
ECC0H non-halogenated flame-retardant polyolefin compounds are ideal for applications that require non-corrosive materials such as mass transit, tunnels, and airports. Originally designed to meet European requirements in the transportation industry, these compounds are used for both sheathing and primary insulation. Specially designed for thin wall extrusion wire and cable applications, ECC0H compounds are low smoke and highly flame-retardant, and will not emit corrosive gasses when burned. Description/Features: - Non-Halogenated
- Low Smoke
- Flame Retardant
Applications: - Thin-wall extrusion applications (Tape, x-web)
Market: Processing Method: TENSILE AND ELONGATION VALUES ARE LARGELY DETERMINED BY PROCESSING PARAMETERS OF THE END USER. NOTE: Tensile property data is from extruded tape 3:1 drawdown ratio and .006 in. NOTE: Dielectric Constant is measured on .085" plaque).PolyOne First Choice Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Dielectric Constant
- Oxygen Index
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|