PolyOne ECCOH™ 1016 Low Smoke Free Of Halogen (LSFOH)
Subcategory: Thermoplastic
Material Notes:
ECC0H 1016 is a low smoke flame retardant zero halogen compound. This product is designed to meet DIN/VDE 0207 p.24 HM2, BS 6724, NF C 32 323 for low voltage cables. ECC0H 1016 combines a good flame retardancy, and chemical and electrical properties. Description/Features: - Low Smoke Flame Retardant Zero Halogen Compound (LSFOH)
Applications: Market: PolyOne First ChoiceDisclaimer: NOTE: "Pass" on Vertical Burn Test is dependant on cable construction. "Pass" on Smoke Density pertains to test performed on test sheets. Information provided by PolyOne Corporation.
| Available Properties |
- pH
- Mooney Viscosity
- Halogen Content
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength @ Yield
- Elongation at Break
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dissipation Factor
- Maximum Service Temperature, Air
- Oxygen Index
- Appearance
- Cold Impact @ -25°C
- Heat Shock, 1 hr @ 150° C
- Hot Pressure Test
- Immersion- Elo. variation from Orig.
- Immersion- TS variation from Orig.
- Smoke Density
- Toxicity
- Vertical Burn Test
- Water Absorption
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|