PolyOne ECCOH™ 6150 Low Smoke Free Of Halogen (LSFOH)
Subcategory: Thermoplastic
Material Notes:
ECC0H 6150 is a low smoke flame retardant zero halogen compound. This product is designed for insulation of low voltage and communication cables. ECC0H 6150 combines good flame retardancy with outstanding mechanical and enhanced wet electrical properties. 1.5mm² Cu conductor insulated with ECC0H 6150 passes IEC 60332-1. It can be processed up to 230°C on PVC extruders. Description/Features: - Low Smoke Flame Retardant Zero Halogen Compound (LSFOH)
Applications: Market: PolyOne First ChoiceDisclaimer: NOTE: "Pass" on Vertical Burn Test is dependant on cable construction. "Pass" on Smoke Density pertains to test performed on test sheets. Information provided by PolyOne Corporation.
| Available Properties |
- pH
- Mooney Viscosity
- Halogen Content
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength @ Yield
- Elongation at Break
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dissipation Factor
- Maximum Service Temperature, Air
- Oxygen Index
- Shrinkage
- Appearance
- Cold Impact @ -25°C
- Heat Shock, 1 hr @ 150° C
- Hot Pressure Test
- Immersion - Increase in AC Capacity
- Immersion- Elo. variation from Orig.
- Immersion- TS variation from Orig.
- Smoke Density
- Toxicity
- Vertical Burn Test
- Water Absorption
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|