PolyOne Lubri-Tech® PC-20GF/15T FRV0 Polycarbonate (PC), Glass Filled, PTFE Lubricated
Subcategory: Polycarbonate; Thermoplastic; Polymer
Material Notes:
Description/Features: - Glass Fiber Reinforced
- PTFE Lubricated
- 20% Glass Filled
- Flame Retardant
PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Surface Resistivity per Square
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Drying Temperature
- Dry Time
|
|
|
|